Cathodic Protection System for Rehabilitation of Marine Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cathodic Protection System for Rehabilitation of Marine Concrete Structures

Author(s): K. Takewaka and T. Minematsu

Publication: Symposium Paper

Volume: 126

Issue:

Appears on pages(s): 657-678

Keywords: cathodic protection; corrosion; durability; harbor structures; repairs; salt water; General

DOI: 10.14359/3797

Date: 8/1/1991

Abstract:
The impressed current-type of cathodic protection was evaluated for controlling of marine concrete structures as follows: To establish criteria of cathodic protection on marine concrete structures, to develop a system that can distribute current uniformly to all reinforcement, and to investigate the over-protection problem that effects the bonding of reinforcement and durability of anode material. The application of the cathodic protection system for the rehabilitation of a harbor concrete structure in Japan was also examined.