Title: Concrete progress--Worth telling about

Author(s): Walter E. Kunze

Publication: Concrete International

Volume: 9

Issue: 12

Appears on pages(s): 17-22

Keywords: bridges (structures); buildings; concrete construction; reviews; concrete technology; General

DOI:

Date: 12/1/1987

Abstract:
A review of today's many uses of concrete and a look at current advancements on the leading edge of technology are presented.