Concrete Deck Renews Delaware Aqueduct Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Deck Renews Delaware Aqueduct Bridge

Author(s): Fu-Kuei Chang and Edward Cohen

Publication: Concrete International

Volume: 13

Issue: 2

Appears on pages(s): 27-29

Keywords: aqueducts; bridge decks; concrete concstruction; prepact concrete; composite construction (concrete to concrete); history; renovating; General

DOI:

Date: 2/1/1991

Abstract:
Describes renovation of an American civil engineering landmark originally constructed in 1847-48 to carry the Delaware Hudson Canal across the Delaware River. After many years of use as a private highway toll bridge, the structure was closed to vehicular traffic. Renovation included adding a concrete bridge deck to the timber structure