Evaluation of a Deteriorated Post-Tensioned One-Way Slab

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of a Deteriorated Post-Tensioned One-Way Slab

Author(s): Robert Tracy, Steven Crower, and Khadije Zwoer

Publication: Concrete International

Volume: 13

Issue: 6

Appears on pages(s): 27-32

Keywords: concrete slabs; deterioration; evaluation; parking facilities; post-tensioning; reinforcing steels; repairs; General

DOI:

Date: 6/1/1991

Abstract:
Describes the evaluation of a post-tensioned one-way parking garage deck slab supported by a post-tensioned precast beam system. Many deck cables had developed major section loss, particularly at construction joints where intermediate stressing points were located. The investigation concluded that the existing deck could be salvaged by restressing the original cables at a new pour strip constructed to replace the intermediate construction joint.