Condition Surveys of Large Diameter Concrete Lined Tunnels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Condition Surveys of Large Diameter Concrete Lined Tunnels

Author(s): Harry R. Price and Keith M. Swaffer

Publication: Concrete International

Volume: 9

Issue: 6

Appears on pages(s): 58-64

Keywords: concretes; deterioration; tunnel linings; inspection; sewers; surveys; General

DOI:

Date: 6/1/1987

Abstract:
A methodology for performing condition surveys of large diameter concrete-lined tunnels is presented. Possible environmental constraints and causes of concrete lining deterioration are discussed, and case histories of two tunnel inspection programs are reviewed.