Questions and Answers on ASTM A 706 Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Questions and Answers on ASTM A 706 Reinforcing Bars

Author(s): A. L. Felder and D. P. Gustavson

Publication: Concrete International

Volume: 13

Issue: 7

Appears on pages(s): 54-57

Keywords: costs; mechanical properties; reinforcing steels; specifications; standards; General

DOI:

Date: 7/1/1991

Abstract:
Answers questions frequently raised by architects, engineers, and constructors about ASTM A 706 reinforcing bars. A wide range of practical questions are addressed including mechanical properties, weldability, availability, and relative costs.