Title: Mass Transfer of Gas and Water Through Concrete

Author(s): R. H. Mills

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 621-644

Keywords: concrete durability; gases; hydration; nitrogen; permeability; porosity; reinforced concrete; water; water-cement ratio; General

DOI: 10.14359/3652

Date: 4/1/1987

Abstract:
Permeability, a prime factor related to durability of concrete, was measured by water and gas flow in plain and reinforced concrete. The results are discussed in terms of porosity and pore size characteristics as determined by mix proportions and hydration parameters. 617-387 Development of impact-resonant vibration signature for inspection of concrete structures