Research Innovations for Durable Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Research Innovations for Durable Concrete

Author(s): G. M. Idorn, Vagn Johansen and N. Thaulow

Publication: Concrete International

Volume: 14

Issue: 7

Appears on pages(s): 19-24

Keywords: blast furnace slag; cement quality; manufacturing; methods; tests; maturity method; precast concrete; production measurement; General

DOI:

Date: 7/1/1992

Abstract:
Concrete production methods and materials have changed radically during the past decades. Concurrently, laboratory research on concrete and on concrete source materials have been furnished with powerful analytical and testing instrumentation and corresponding basic scientific knowledge. The aim of this paper is to stimulate discussions on how parallel developments in practice and research can be effectively integrated for improved quality management of concrete in production, and for improved performance quality of field concrete.