Title: Non-Chloride Accelerating Admixtures for Early Compressive Strength

Author(s): Ken Rear and David Chin

Publication: Concrete International

Volume: 12

Issue: 10

Appears on pages(s): 55-58

Keywords: accelerating agents; admixtures, age-strength relation; compressive strength; concretes; tests; General

DOI:

Date: 10/1/1990

Abstract:
Provides an overview of three different types of nonchloride admixtures that can be used in concrete, and describes the type of early strength results that can be expected from their use.