Monitoring System for the Corrosion Risk of Steel in Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Monitoring System for the Corrosion Risk of Steel in Concrete Structures

Author(s): Peter Schiessl and Michael Raupach

Publication: Concrete International

Volume: 14

Issue: 7

Appears on pages(s): 52-55

Keywords: carbonation; chlorides; corrosion; cover; reinforced concrete; General

DOI:

Date: 7/1/1992

Abstract:
A permanent corrosion-monitoring system has been developed that indicates the corrosion risk for the reinforcement in concrete structures. This system enables the owner to take preventive protection measures before damages occur. Sensors for the system were developed by the Institute for Building Materials Research at TH Aachen, Germany. The electronic equipment for measuring and software for analysis of the data were developed by the Company for Sensors and Prestressing Techniques in Cologne, Germany.