Concrete and the Infrastructure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete and the Infrastructure

Author(s): Mark J. Sisinyak

Publication: Concrete International

Volume: 9

Issue: 6

Appears on pages(s): 19-22

Keywords: bridges (structures); buildings; concrete pavements; evaluation; hydraulic structures; maintenance; renovating; repairs; research; General

DOI:

Date: 6/1/1987

Abstract:
Describes a Corps of Engineers research program--Repair, Evaluation, Maintenance, and Rehabilitation--initiated to identify and develop cost-effective technology to maintain and/or extend the service life of the infrastructure. Studies of several problem areas involving concrete structures and technology transfer efforts are highlighted.