Title: LMC Overlay for O'Hare Airport Parking Garage Roof

Author(s): Lou Kuhlmann

Publication: Concrete International

Volume: 13

Issue: 8

Appears on pages(s): 25-27

Keywords: latex (plastic); parking facilities; plastics, polymers, and resins; polymer concrete; protective coatings; resurfacing; General

DOI:

Date: 8/1/1991

Abstract:
Called the world's largest garage, the six-level public parking structure at Chicago's O'Hare International Airport is also one of the busiest. After 20 years of service, cracking and spalling of the roof deck caused the city to restore the deck using latex-modified concrete.