Placing Specialized Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Placing Specialized Concrete

Author(s): Kenneth L. Saucier

Publication: Concrete International

Volume: 12

Issue: 6

Appears on pages(s): 46-50

Keywords: concretes; placing; resurfacing; roller-compacted concrete; shotcrete; General

DOI:

Date: 6/1/1990

Abstract:
Innovative placement methods for new and specialized types of concrete are described. Typical applications are roller-compacted concrete, frost-resistant shotcrete, cohesive underwater concrete, overlays, and mass-produced concrete mattresses. The use of conventional concrete is also benefitting from new systems, patents, and improvements to established placement techniques.