Prestressed Concrete Bridges in Adverse Environments

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prestressed Concrete Bridges in Adverse Environments

Author(s): Vladamir Novokshchenov

Publication: Concrete International

Volume: 13

Issue: 5

Appears on pages(s): 43-48

Keywords: bridges (structures); chlorides; corrosion; cover; environments; failure; prestressed concrete; General

DOI:

Date: 5/1/1991

Abstract:
Presents the results of a literature survey of prestressing steel failure in bridge members exposed to potentially aggressive environments. The main cause of corrosion of prestressing tendons is the ingress of moisture laden with corrosion-inducing agents. Brittle failure of reinforcing steel can occur due to pitting corrosion and two types of stress corrosion cracking (hydrogen embrittlement and fatigue corrosion).