Modifying Bridges with CLSM

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modifying Bridges with CLSM

Author(s): Jay Goldbaum, William Hook, and Don A. Clem

Publication: Concrete International

Volume: 19

Issue: 5

Appears on pages(s): 44-47

Keywords: backfilling; bridges; low-strength materials; quality control

DOI:

Date: 5/1/1997

Abstract:
The purpose of this article is to document the use of controlled low-strength material (CLSM) as a culvert backfill to convert substandard bridge structures to an on-grade roadway over newly placed culverts. Subjects covered include the history of CLSM in Colorado, design considerations, cost and schedule considerations, mix designs, construction considerations, quality control.