Nondestructive Testing for Repair and Rehabilitation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Nondestructive Testing for Repair and Rehabilitation

Author(s): Larry D. Olson and Clifford C. Wright

Publication: Concrete International

Volume: 12

Issue: 3

Appears on pages(s): 58-64

Keywords: dynamic characteristics; evaluation; foundations; measurement; nondestructive tests; pavements; quality assurance; General

DOI:

Date: 3/1/1990

Abstract:
Case histories are presented to illustrate quality assurance and forensic applications of nondestructive testing and evaluation for the construction industry. The sonic, seismic, and vibration methods described are based on measurement of wave-propagation behavior. These measurements provide data on dynamic properties that are directly and indirectly related to physical conditions of the system being tested. They typically provide engineers with critical data that cannot be obtained economically from traditional destructive test methods.