Tendon Prestressed Concrete Tanks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tendon Prestressed Concrete Tanks

Author(s): Steven R. Close and Ib Falk Jorgensen

Publication: Concrete International

Volume: 10

Issue: 2

Appears on pages(s): 24-29

Keywords: circular prestressing; post-tensioning; prestressed concrete; reinforced concrete; storage tanks; subsurface structures; water tanks; tanks (containers); General

DOI:

Date: 2/1/1988

Abstract:
The advantages and applications of cast-in-place post-tensioned concrete tanks are discussed. Proper design details and construction methods can make these tanks advantageous in a wide variety of circumstances, especially when the tank is to be buried.