Microcomputer-Aided Design of Reinforced and Prestressed Concrete Elements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Microcomputer-Aided Design of Reinforced and Prestressed Concrete Elements

Author(s): F. C. Filippou

Publication: Symposium Paper

Volume: 111

Issue:

Appears on pages(s): 1-16

Keywords: axial loads; beams (supports); bending moments; microcomputers; prestressed concrete; reinforced concrete; structural design; General

DOI: 10.14359/3592

Date: 12/1/1988

Abstract:
Potential advantages of using electronic spreadsheets in advanced reinforced and prestressed concrete design are presented. The power of this tool is demonstrated through a series of examples, including the moment-curvature relation of reinforced and prestressed concrete beams, the axial load-uniaxial and biaxial bending moment interaction diagram of reinforced concrete sections, and the tendon layout of simply supported beams prestressed with draped or straight tendons.