Heavy Duty Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Heavy Duty Pavements

Author(s): Ronald L. Hutchinson, Steven A. Ragan, and David W. Pittman

Publication: Concrete International

Volume: 9

Issue: 2

Appears on pages(s): 55-61

Keywords: batching; consolidation; conveying; freeze-thaw durability; joints (junctions); load transfer; mixing; mix proportioning; pavements; quality control; roller-compacted concrete; thickness; General

DOI:

Date: 2/1/1987

Abstract:
The Corps of Engineers' initial interest in roller-compacted concrete (RCC) was for use in mass concrete construction. Recently, however, the Corps has also begun using RCC for construction of heavy-duty pavements for low-speed traffic. There pavements must be able to withstand fuels, oils, deicing solutions, washwater, and other chemicals from routine maintenance of military equipment. The U.S. Army Engineer Waterways Experiment Station is currently conducting research into RCC pavement mixture proportioning, thickness, design, construction, quality assurance testing, and frost resistance. The results of this research will be used to develop guidance to assist Corps field offices in the design and construction of RCC pavements.