Triaxial Behavior of High-Strength Concrete and Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Triaxial Behavior of High-Strength Concrete and Mortar

Author(s): Claus Vestergaard Nielsen

Publication: Materials Journal

Volume: 95

Issue: 2

Appears on pages(s): 144-151

Keywords: cohesion; confinement; Coulomb failure criterion; cracked strength; dilatation; friction; high-strength mortar/concrete; steel fibers; triaxial compression; ultimate strains;

DOI: 10.14359/359

Date: 3/1/1998

Abstract:
Triaxial axisymmetrical compression tests were performed on cylinders of ultra-high-strength mortar. The matrix was reinforced with straight steel fibers (6 percent by volume) and had a uniaxial compressive strength of 165 MPa (24 ksi). Comparisons were made with similar triaxial strength results on plain high-strength concrete (HSC) and mortar. The Coulomb friction failure criterion was applied to fit the data. The brittle compressive failure of HSC was reflected in the appearance of the failure criterion. The angle of friction governing the behavior under small confinement pressures equaled 51 deg instead of 37 deg, which is typically seen for normal strength concrete. Under increasing confinement pressures the angle of friction reduced to 30 deg due to the fact that the crack growth in HSC is only slightly influenced by the aggregate. Finally, the axial and lateral strains corresponding to the ultimate triaxial load were assessed in order to predict the deformations of confined HSC.