Title: High Early Strength Blended-Cement Wet-Mix Shotcrete

Author(s): Dudley R. Morgan

Publication: Concrete International

Volume: 13

Issue: 5

Appears on pages(s): 35-39

Keywords: blended cements; compressive strength; flexural strength; freeze-thaw durability; mix proportioning; performance tests; General

DOI:

Date: 5/1/1991

Abstract:
Evaluates the performance of wet-mix shotcrete made with a new high early strength, blended cement. Shotcrete made with this new cement demonstrates good supply and application characteristics, impressive early and later age strength development, and good durability in aggressive exposure conditions.