Title: Guide for Concrete Inspection

Author(s): ACI Committee 311

Publication: Materials Journal

Volume: 85

Issue: 4

Appears on pages(s): 303-313

Keywords: acceptability; concretes; contractors; evaluation; field tests; inspection; laboratories; measurement; quality control; tests; General

DOI: 10.14359/3578

Date: 7/1/1988

Abstract:
Guide discusses the need for inspection of concrete construction and other related activities, the types of inspection activities involved, and the responsibilities of various individuals and organizations involved in these activities. Field testing activities are considered to be part of the inspection program. The guide presents recommended plans for the various types of inspection activities and means of implementing the plans. Recommended minimum levels of inspection for various purposes and various types of projects are given.