Automatic Quantitative Image Analysis System for Cement and Concrete Research

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Automatic Quantitative Image Analysis System for Cement and Concrete Research

Author(s): Dexiang Shi

Publication: Symposium Paper

Volume: 106

Issue:

Appears on pages(s): 139-158

Keywords: algorithms; cements; computer programs; concretes; measurement; microscopy; particle size distribution; General

DOI: 10.14359/3562

Date: 6/1/1988

Abstract:
An automatic quantitative image analysis (AQIA) software system has been developed to quantify constituents in multiple phase materials, such as hardened cement and concrete. Some major features of AQIA are presented. The applications of AQIA to cement and concrete research are explored. The system is expected to provide a more versatile, and more reliable means than the manual microscope examination. It is much less expensive than existing hardware-type image analyzers, and specially designed for materials use.