Title: Structural Integrity of a Damaged Building

Author(s): Jihad B. Bahlis and M. Saeed Mirza

Publication: Concrete International

Volume: 10

Issue: 4

Appears on pages(s): 35-37

Keywords: columns (supports); damage; dynamic loads; explosions; finite element method; flat concrete slabs; high-rise buildings; shearwalls; load tests (structural); reinforced concrete; repairs; General

DOI:

Date: 4/1/1988

Abstract:
The structural integrity and safety of a 24-story reinforced concrete building damaged by an explosion are investigated using finite element analysis and load tests. Repair of the damaged areas is described.