Computer aided equipment selection for concrete placing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computer aided equipment selection for concrete placing

Author(s): SABAH ALKASS and APRAHAM ARONIAN

Publication: Concrete International

Volume: 12

Issue: 12

Appears on pages(s): 39-45

Keywords: computer programs; concrete construction; concretes; construction equipment; costs; expert systems; placing; quality control; General

DOI:

Date: 12/1/1990

Abstract:
A prototype integrated computer system has been developed to assist in planning and controlling concrete placing operations. Developing the system has illustrated the complex managerial decisions that must be made during the process. The system has considerable value in assisting less experienced personnel in reaching such decisions. The program is an expert system designed to aid in equipment selection.