Abstract of: Texturing Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Abstract of: Texturing Concrete Pavements

Author(s): ACI Committee 325

Publication: Concrete International

Volume: 10

Issue: 8

Appears on pages(s): 50-52

Keywords: concrete finishes (hardened concrete); concrete pavements; concrete finishing (fresh concrete); maintenance; measurement; texture; skid resistance; General

DOI:

Date: 8/1/1988

Abstract:
Increased traffic volumes and speeds have increased the need for improved skid resistant surfaces. The emphasis has been to improve skid resistance by creating new surfaces that increase the "macrotexture" of the concrete pavement. These textures are created by forming deeper textures in plastic concrete during finishing operations or by sawing grooves in the hardened concrete of existing pavements with cutting heads composed of a number of circular diamond saw blades.