Title: Simplifying Concrete Mix Design With the PC

Author(s): Kurt F. Peyfuss

Publication: Concrete International

Volume: 12

Issue: 12

Appears on pages(s): 47-49

Keywords: aggregates; computer programs; concretes; microcomputers; mix proportioning; pumped concrete; General

DOI:

Date: 12/1/1990

Abstract:
Describes a spreadsheet using Lotus "Symphony" that can be used to calculate quantities of aggregates, cement, water, and admixtures from entered mix specifications.