Computer-Aided Cusum Analysis and Evaluation of Concrete Strength Test Results

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Computer-Aided Cusum Analysis and Evaluation of Concrete Strength Test Results

Author(s): H. W. Chung and Stephen Hung

Publication: Concrete International

Volume: 10

Issue: 6

Appears on pages(s): 58-61

Keywords: compressive strength; computer programs; concrete construction; evaluation; quality assurance; quality control; statistical analysis; General

DOI:

Date: 6/1/1988

Abstract:
The role of the microcomputer in statistical control of concrete, particularly at the site office, is discussed, and the use of cusum analysis in determining whether a concrete production process is in statistical control is described.