Why Vibrate?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Why Vibrate?

Author(s): H. A. Welton

Publication: Symposium Paper

Volume: 96

Issue:

Appears on pages(s): 119-124

Keywords: capillarity; concretes; consolidation; mixing; mix proportioning; placing; porosity; vibration; voids; water; Manufacturing

DOI: 10.14359/3507

Date: 1/1/1987

Abstract:
A brief discussion of consolidation of concrete aimed toward the users of concrete is presented to encourage the use of vibration in improving the quality of the finished product. Significant points leading to successful consolidation of quality concrete include the interrelationship of proportioning, mixing, placement, and application of the vibrator to break down mechanical stacking, eliminate unintentional air voids, reduce residual water content, and achieve densification and enhancement of the micro-structure of the concrete.