High-Strength Concrete in Melbourne, Australia

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Strength Concrete in Melbourne, Australia

Author(s): Ian Burnett

Publication: Concrete International

Volume: 11

Issue: 4

Appears on pages(s): 17-25

Keywords: columns (supports); concrete slabs; high-strength concretes; pumped concrete; slipform construction; walls; General

DOI:

Date: 4/1/1989

Abstract:
Describes the specification, supply, control, and construction of three large structures in downtown Melbourne, Australia, using 60 and 65 Mpa (8700 and 9425 psi) concrete. The advantages of high-strength concrete--reduction in member size, thus increasing rentable space; early stripping of formwork; greater stiffness; and reduced axial shortening of compression elements--are discussed, as are cost studies, test programs, supply plants and delivery, materials, mix proportions, placing and compaction, and compression testing and quality control.