Constructing a Superflat Concrete Floor Slab

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Constructing a Superflat Concrete Floor Slab

Author(s): Don Gehring

Publication: Concrete International

Volume: 11

Issue: 6

Appears on pages(s): 28-33

Keywords: concrete slabs; floors; heavy-duty floors; measurement; tolerances (mechanics); Construction

DOI:

Date: 6/1/1989

Abstract:
Describes the construction of a warehouse floor that includes post-tensioned slabs with specified minimum flatness of F 100, and explains the techniques necessary for meeting superflat floor slab specifications.