Title: Thin Bonded Concrete Overlay on a City Street

Author(s): Arthur R. Beck

Publication: Concrete International

Volume: 11

Issue: 5

Appears on pages(s): 39-47

Keywords: bonding; concrete construction; resurfacing; streets; thickness; Construction

DOI:

Date: 5/1/1989

Abstract:
Construction procedures and test results on a thin-bonded concrete overlay on a city street in Richardson, Texas, are described. Citizen complaints about the messiness of asphaltic concrete and its making the neighborhood look old prompted the city to explore this method of pavement rehabilitation.