Inspection of Unbonded Tendons

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Inspection of Unbonded Tendons

Author(s): Daniel W. Falconer and Philip W. Wilson

Publication: Concrete International

Volume: 10

Issue: 2

Appears on pages(s): 53-56

Keywords: beams (supports); concrete slabs; foundations; inspection; post-tensioning; prestressed concrete; unbonded prestressing; Construction

DOI:

Date: 2/1/1988

Abstract:
Post-tensioning delivers an active force. When post-tensioning strands are improperly placed, the active force can result in local failures such as blowouts or breakouts where the strand actually pulls through the concrete. These and other problems are dangerous when they occur and very difficult and expensive to repair. Many of these problems can be prevented by good inspection.