Tips for Post-Tensioning

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tips for Post-Tensioning

Author(s): Daniel W. Falconer

Publication: Concrete International

Volume: 10

Issue: 2

Appears on pages(s): 36-39

Keywords: concrete durability; detailing; economics; parking facilities; post-tensioning; structural design; unbonded prestressing; Construction

DOI:

Date: 2/1/1988

Abstract:
A successful post-tensioned parking garage is obtained largely through well-conceived details. An overall understanding of how post-tensioning acts on the structure will result in a durable and economical structure with very few problems.