Durability of Prestressed Concrete Tanks Constructed With Dry-Mix Shotcrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability of Prestressed Concrete Tanks Constructed With Dry-Mix Shotcrete

Author(s): Morris Schupack and Randall W. Poston

Publication: Concrete International

Volume: 11

Issue: 10

Appears on pages(s): 51-55

Keywords: corrosion; delaminating; deterioration; durability; freeze-thaw durability; prestressed concrete; prestressing steels; shotcrete; tanks (containers); Construction

DOI:

Date: 10/1/1989

Abstract:
Presents observations regarding the long-term durability of dry-mixed shotcrete used in the construction of prestressed concrete tanks. In general, shotcrete performance in prestressed concrete tanks constructed over 30 years ago has been good in the aggressive freeze-thaw environment of the northeast United States. Problems that have been observed, primarily in domes, are attributed to poor construction practice, and not to a lack of inherent durability of shotcrete.