Repair of Red Rock Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repair of Red Rock Dam

Author(s): Billy D. Neely and Jerry Wickersham

Publication: Concrete International

Volume: 11

Issue: 10

Appears on pages(s): 36-39

Keywords: admixtures; concretes; pumping; repairs; underwater construction; Construction

DOI:

Date: 10/1/1989

Abstract:
An eroded end sill at Red Rock Dam on the Des Moines River in south central Iowa was repaired using a flowable, cohesive concrete containing an antiwashout admixture. The concrete was pumped into place while a diver guided the discharge end of the pump line. Article presents a case history of a successful dam repair using underwater concreting techniques.