Low Pressure Grouting of Polyethylene Pipe

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Low Pressure Grouting of Polyethylene Pipe

Author(s): Patrick J. Stephens

Publication: Concrete International

Volume: 11

Issue: 10

Appears on pages(s): 45-46

Keywords: cellular concretes; grout; grouting; pumped concrete; renovating; repairs; sewers; Construction

DOI:

Date: 10/1/1989

Abstract:
Describes the application of low-density cellular foam concrete grout in backfilling high-density polyethylene pipe liners used to rehabilitate sewers.