Changing the Shape of Wastewater Treatment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Changing the Shape of Wastewater Treatment

Author(s): Gerhard Sutter

Publication: Concrete International

Volume: 12

Issue: 11

Appears on pages(s): 21-25

Keywords: concrete construction; digesters; formwork (construction); prestressed concrete; tanks (containers); waste treatment; water treatment; Construction

DOI:

Date: 11/1/1990

Abstract:
Describes design and construction of several prestressed concrete egg-shaped sludge digesters under construction at two German wastewater treatment plants. Article focuses on the prefabricated and reusable formwork designed for construction of the tanks.