Bridge of Joigny

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bridge of Joigny

Author(s): Yves Malier, Didier Brazillier, and Stephane Roi

Publication: Concrete International

Volume: 13

Issue: 5

Appears on pages(s): 40-42

Keywords: bridges (structures); high-strength concretes; prestressed concrete; Construction

DOI:

Date: 5/1/1991

Abstract:
The French Ministry of Public Works and the National Project on New Concretes team constructed an experimental prestressed bridge using high-strength concrete (60 MPa). Their goal was to prove high-strength structures could be built using local aggregates and ready-mixed concrete plants.