Shore and Reshore Scheduling Using a Microcomputer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shore and Reshore Scheduling Using a Microcomputer

Author(s): N. J. Gardner and A. Muscati

Publication: Concrete International

Volume: 11

Issue: 8

Appears on pages(s): 32-36

Keywords: age-strength relation; computer programs; concrete construction; flat concrete slabs; form removal; formwork (construction); loads (forces); multistory buildings; safety; shoring; Construction

DOI:

Date: 8/1/1989

Abstract:
A computer program that analyzes the safety of proposed construction schedules for multistory flat slab-type structures is described. The program, which is suitable for microcomputers, allows the user to input a proposed erection schedule and determine if it is appropriate. Alternatively, the number of forms and reshores can be input and the stripping and casting schedule calculated, or the stripping and casting times input and acceptable form/reshore combinations determined.