Equivalent Frame Analysis of Concrete Buildings During Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Equivalent Frame Analysis of Concrete Buildings During Construction

Author(s): Pericles C. Stivaros and Grant T. Halvorson

Publication: Concrete International

Volume: 13

Issue: 8

Appears on pages(s): 57-62

Keywords: concrete construction; failure; flat concrete slabs; formwork (construction); loads (forces); multistory buildings; punching shear; safety; shoring; structural analysis; Construction

DOI:

Date: 8/1/1991

Abstract:
The equivalent frame method (EFM) has been widely accepted as a satisfactory design procedure for two-way reinforced concrete slab systems. The same method and principles can also apply to the analysis of reinforced concrete buildings during construction, while formwork and shoring systems are still in place. The EFM-based analytical procedure is demonstrated by its application to the 1981 construction failure of the Harbour Cay Condominium.