Title: Elastomeric Coatings for Concrete and Masonry

Author(s): RobertT L. Kneur and Luis M. Calvo

Publication: Concrete International

Volume: 12

Issue: 4

Appears on pages(s): 54-55

Keywords: coatings; concrete construction; plastics, polymers and resins; masonry; protective coatings; Construction

DOI:

Date: 4/1/1990

Abstract:
Describes the technology for producing a flexible coating system for concrete and masonry that is intended for use in areas where cracking or crazing might occur in an inflexible coating.