An Airport Apron and a County Road

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Airport Apron and a County Road

Author(s): Jory M. Abrams and Jerry L. Jackshaw

Publication: Concrete International

Volume: 9

Issue: 2

Appears on pages(s): 30-36

Keywords: aggregates; airports; aprons; bituminous concretes; cements; concrete pavements; curing; mix proportioning; roller compacted concrete; roads; tests; Construction

DOI:

Date: 2/1/1987

Abstract:
Presents examples of two uses of roller-compacted concrete pavement: an airport apron and a county road improvement. The planning, design, construction, and testing processes are described, as well as details of the mix proportions and curing methods.