Mechanized Installation of Concrete Block Paving

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanized Installation of Concrete Block Paving

Author(s): David R. Smith

Publication: Concrete International

Volume: 9

Issue: 7

Appears on pages(s): 37-40

Keywords: concrete blocks; installing; pavements; paving blocks; precast concrete; roads; Construction

DOI:

Date: 7/1/1987

Abstract:
Mechanized methods for installing concrete block paving (CBP), originally developed in Europe, have been introduced to North America. This mechanized technology can reduce the cost of CBP enough to make it competitive with conventional pavements. A recent pavement project in Dayton, Ohio, demonstrated the time and cost savings that are possible.