Abstract:
Described rehabilitation of the headwork structures for a power-generating station. The project included building and removing a cofferdam along the existing ice diverter; dewatering the inner and outer forebays; structurally upgrading the ice diverter, outer forebay spillway, gatehouse apron, and maingate sills; constructing new trash racks; demolishing an old screenhouse structure; building a scenic walkway; and cleaning debris from the forebay.