Zilwaukee Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Zilwaukee Bridge

Author(s): Robert I. Pearson

Publication: Concrete International

Volume: 10

Issue: 5

Appears on pages(s): 68-75

Keywords: bridges (structures); concrete construction; post-tensioning; load tests (structural); precast concrete; repairs; segmental construction; safety; Construction

DOI:

Date: 5/1/1988

Abstract:
The new eight-lane Zilwaukee Bridge in Michigan replaces an aging four-lane drawbridge that was a hazard to both navigation and freeway traffic. The new post-tensioned, segmental, precast concrete box-girder structure actually two bridges, each measuring 1.5 miles (2.4 km) long and 125 ft (38 m) high] was constructed using the balanced cantilever method.