Alkalicarbonate Rock Reaction at Center Hill Dam, Tennessee

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Alkalicarbonate Rock Reaction at Center Hill Dam, Tennessee

Author(s): Thomas L. Hugenberg

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 1883-1902

Keywords: alkali-carbonate reactions; bridges (structures); concrete cores; concrete dams; evaluation; expansion; repairs; spillways; tests; Construction

DOI: 10.14359/3330

Date: 4/1/1987

Abstract:
Expansion of the concrete at Center Hill Dam during its 38-year service life resulted in binding of the spillway gates and closing of the expansion joints in the bridge spans in 1983. An extensive laboratory and field investigation identified an alkali-carbonate rock reaction as the cause of expansion. Shortening of the spillway gates and bridge spans in 1985 remedied the operational deficiencies.