New Materials for Prestressing and Monitoring Heavy Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: New Materials for Prestressing and Monitoring Heavy Structures

Author(s): Reinhard Wolff and Hans-Joachin Miessler

Publication: Concrete International

Volume: 11

Issue: 9

Appears on pages(s): 86-89

Keywords: bridges (structures); glass fibers; monitors; polyester resins; prestressed concrete; prestressing; Construction

DOI:

Date: 9/1/1989

Abstract:
Prestressing tendons made of glass fiber composite material were used on the Ulenbergstresse Bridge in Dusseldorf in 1986. The composite material used consists of Type E glass fibers and a polyester resin matrix coated on-line with polyamide for protection against mechanical or chemical attack.