Abstract of: Guide for Design and Construction of Parking Lots

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Abstract of: Guide for Design and Construction of Parking Lots

Author(s): ACI Committee 330

Publication: Concrete International

Volume: 10

Issue: 8

Appears on pages(s): 36-42

Keywords: air entrainment; coatings; compacting; concrete construction; concrete durability; concrete pavements; concrete slabs; curing; dowels; drainage; economics; finishing; joints (junctions); joint sealers; soils; loads (forces); load transfer; maintenance; p

DOI:

Date: 8/1/1988

Abstract:
Reports the current knowledge and practices for the design, construction, and maintenance of concrete parking lots placed at ground level.