Seattle Sewer Rehabilitation

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seattle Sewer Rehabilitation

Author(s): Robert I. Pearson

Publication: Concrete International

Volume: 9

Issue: 4

Appears on pages(s): 32-34

Keywords: cellular concretes; grout; grouting; pumped concrete; renovating; repairs; sewers; tunnels; Construction

DOI:

Date: 4/1/1987

Abstract:
Cellular foam concrete grout was pumped a record distance in the rehabilitation of a 95-year-old double-brick lined sewer tunnel.